Properties
  • Good resistance to aggressive environment
  • Low hydration temperature
  • Slow strength buildup
  • Light colored cement – free of fly ash
  • Develops resistance to chloride penetration
  • Improves concrete spreading in a sulfate environment
Applications
  • Structural elements – high CAME
  • Stabilization of soil contaminated with chlorides and sulfates
  • Enables transfer of concrete admixtures via pumps
  • Pouring shell walls near the seaside – light colored concrete
  • Large-scale pourings- mass concrete
  • Pouring of floors and subterranean structures
  • Pouring water tanks, pools and pipes – high impermeability in suitable concrete admixtures
  • Oxygenation pools and wastewater treatment facilities
  • Improvement of elements that have been damaged by an aggressive environment
Binder type: Portland cement
  • Definition (IS 1 EN 197-1): CEM III 42.5 N/B slag cement
  • Packaging/sale configuration: Bulk
  • Main ingredients: Slag (minimum 65%), clinker
  • Test and labeling method – standard: IS 1 – July 2002 196 1-7 EN
Compression load (Newton/sq.m)
Standard requirement Average value
2 10
28 42.5
Binding time, minutes
Standard requirement Average value
Minimum 60
Maximum 600
Minutes
  • Specific surface area (sq.cm/gram): 5,300
  • Bulk spatial weight (kg/cu.m): 1,100 – 1,350
  • Density (kg/cu.m): 2,880
Compressive strength - MPa slump cone
graph